Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mitsui AURUM® PL450C Polyimide  (discontinued **)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Unfilled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mitsui AURUM® PL450C Polyimide  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURUM PL450C offers a unique balance of mechanical and thermal properties for superior performance in demanding automotive, business machinery, industrial equipment, aerospace, and semiconductor equipment applications. AURUM exhibits outstanding resistance to chemicals and radiation, a low coefficient of thermal expansion, ultrahigh purity, low outgassing in a vacuum, excellent electrical properties, and flame resistance. AURUM PL450C can be conventionally extruded to produce high performance wire & cable insulation, thin-wall tubing, and fiber.Applications: AURUM PL450C injection molded components are excellent replacements for metals, ceramics, and other plastics. High performance AURUM PL450C parts include heat-resistant gears, seals, ferrules and other fasteners, coil bobbins, semiconductor manufacturing and handling equipment components, and thermal and electrical insulators. Products produced from extruded AURUM PL450C resin include thin-wall tubing, wire and cable insulation, monofilament, and rod stock shapes.Information provided by DuPont
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Water Absorption 0.34 %
0.34 %
24 hrs @ 73°F; ASTM D570
Moisture Absorption at Equilibrium 0.24 %
0.24 %
73°F; 60 RH, 24hrs
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Melt Flow 4.5 - 7.5 g/10 min

@Load 1.05 kg,
Temperature 400 °C
4.5 - 7.5 g/10 min

@Load 2.31 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 92.18 MPa
13370 psi
ASTM D638
57.9 MPa

@Temperature 149 °C
8400 psi

@Temperature 300 °F
ASTM D638
Elongation at Yield 90 %
90 %
ASTM D638
90 %

@Temperature 149 °C
90 %

@Temperature 300 °F
ASTM D638
Modulus of Elasticity 2.76 GPa
400 ksi
ASTM D882
Flexural Strength 137 MPa
19900 psi
ASTM D790
88.3 MPa

@Temperature 149 °C
12800 psi

@Temperature 300 °F
ASTM D790
Flexural Modulus 2.943 GPa
426.8 ksi
ASTM D790
2.550 GPa

@Temperature 149 °C
369.9 ksi

@Temperature 300 °F
ASTM D790
Compressive Strength 76.5 MPa

@Temperature 149 °C
11100 psi

@Temperature 300 °F
JIS K7208
119.7 MPa

@Temperature 22.8 °C
17360 psi

@Temperature 73.0 °F
JIS K7208
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 22.8 °C
30.0 µin/in-°F

@Temperature 73.0 °F
MD; ASTM D696
54.0 µm/m-°C

@Temperature 73.0 °C
30.0 µin/in-°F

@Temperature 163 °F
TD; ASTM D696
Specific Heat Capacity 1.00 J/g-°C
0.240 BTU/lb-°F
DSC
1.004 J/g-°C

@Temperature 100 °C
0.2400 BTU/lb-°F

@Temperature 212 °F
DSC
1.423 J/g-°C

@Temperature 300 °C
0.3400 BTU/lb-°F

@Temperature 572 °F
DSC
Thermal Conductivity 0.174333 W/m-K
1.20987 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 388 °C
730 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 238 °C
460 °F
ASTM D648
Glass Transition Temp, Tg 250 °C
482 °F
DSC
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
5VA

@Thickness 2.00 mm
5VA

@Thickness 0.0787 in
Oxygen Index 47 %

@Thickness 3.20 mm
47 %

@Thickness 0.126 in
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cm
1.00e+17 - 1.00e+18 ohm-cm
ASTM D257
Surface Resistance 1.00e+17 - 1.00e+18 ohm
1.00e+17 - 1.00e+18 ohm
ASTM D257
Dielectric Constant 3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
ASTM D150
3.2

@Frequency 1000 Hz
3.2

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.00090

@Frequency 1000 Hz
0.00090

@Frequency 1000 Hz
ASTM D150
0.0034

@Frequency 1e+6 Hz
0.0034

@Frequency 1e+6 Hz
ASTM D150