Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Solvay Specialty Polymers
Trade Name Hyflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, inherent flame resistance, low surface energy, and exceptional dielectric properties. Hyflon® PFA resins have been designed to retain their properties over a wide range of temperatures from cryogenic to 250-260°C (482-500°F) and are the material of choice in applications such as linings in the Chemical Process Industry, specialty cables, semiconductor industry, aerospace, and other challenging industries.Features: Flame Retardant; High Heat Resistance; Low Flow; Semi CrystallineUses: Aerospace Applications; Cable Jacketing; Liners; Piping; Semiconductor Molding CompoundsAdditional Properties: Crystallization Heat - DSC 18.0 to 26.0 J/g; Flex Life - ASTM D2176 (300.0 µm): 4.0E+3 to 6.0E+3 Cycles; Heat of Fusion - DSC 18.0 to 26.0 J/gInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 2.13 - 2.18 g/cc
0.0770 - 0.0788 lb/in³
ASTM D792
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
ASTM D2240
Tensile Strength at Break >= 21.0 MPa
>= 3050 psi
ASTM D638
Elongation at Break >= 280 %
>= 280 %
ASTM D638
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Specific Heat Capacity 0.900 - 1.10 J/g-°C
0.215 - 0.263 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.200 W/m-K

@Temperature 40.0 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 104 °F
ASTM C177
Melting Point 280 - 290 °C
536 - 554 °F
DSC
Crystallization Temperature 255 - 265 °C
491 - 509 °F
Peak; ASTM D3418
Maximum Service Temperature, Air 250 °C
482 °F
Continuous Use
Flammability, UL94 V-0
V-0
Oxygen Index 95 %
95 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+17 ohm
>= 1.00e+17 ohm
ASTM D257
Dielectric Constant 2.0

@Frequency 100000 Hz
2.0

@Frequency 100000 Hz
ASTM D150
2.0

@Frequency 50.0 Hz
2.0

@Frequency 50.0 Hz
ASTM D150
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
ASTM D149
Dissipation Factor <= 0.00050

@Frequency 100000 Hz
<= 0.00050

@Frequency 100000 Hz
ASTM D150
<= 0.00050

@Frequency 50.0 Hz
<= 0.00050

@Frequency 50.0 Hz
ASTM D150
Descriptive Properties Value Comments
Agency Ratings ASTM D 3307, Type VII; UL 758
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Compression Molding; Extrusion
Injection Molding; Resin Transfer Molding