| Category | Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP), Molded, Fiber Filled , Filled/Reinforced Thermoset |
| Manufacturer | Cosmic Plastics |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.52 g/cc | 0.0549 lb/in³ | |
| Apparent Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | |
| Water Absorption | 0.35 % | 0.35 % | 48 hrs, 50°C |
| Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | typical. |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 25.0 - 34.0 MPa | 3630 - 4930 psi | |
| Flexural Strength | 71.0 MPa | 10300 psi | |
| Compressive Strength | 165 MPa | 23900 psi | |
| Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 42.0 µm/m-°C @Temperature 20.0 °C |
23.3 µin/in-°F @Temperature 68.0 °F |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | 280 °F | Heat Distortion temperature |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | |
| Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
| Dielectric Constant | 3.3 @Frequency 1e+6 Hz |
3.3 @Frequency 1e+6 Hz |
Wet |
| 3.4 @Frequency 1000 Hz |
3.4 @Frequency 1000 Hz |
Wet | |
| Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
| Dissipation Factor | 0.015 @Frequency 1e+6 Hz |
0.015 @Frequency 1e+6 Hz |
Wet |
| 0.022 @Frequency 1000 Hz |
0.022 @Frequency 1000 Hz |
Wet | |
| Arc Resistance | 125 sec | 125 sec |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |