Processing Properties Metric English Comments
Melt Temperature 199 - 204 °C
390 - 399 °F
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Wire & Cable JA612EA Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 163 - 204 °C
325 - 399 °F
PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Melt Temperature 182 - 204 °C
360 - 399 °F
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE)
Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer..
Melt Temperature 182 - 204 °C
360 - 399 °F
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize..
Melt Temperature 182 - 204 °C
360 - 399 °F
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl..
Melt Temperature 191 - 204 °C
376 - 399 °F
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Dry Blend E7130 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible A7501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible)
This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible G92D Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R132BE Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R1765K Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R999A Black Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible B6DB1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R252AE Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Melt Temperature 191 - 204 °C
375 - 400 °F
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase
Melt Temperature 188 - 204 °C
370 - 399 °F
Molding
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ..
Melt Temperature 188 - 204 °C
370 - 399 °F
Molding
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
Melt Temperature 188 - 204 °C
370 - 399 °F
Extrusion
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product ..
Melt Temperature 166 - 204 °C
330 - 400 °F
M. Holland Company MAGMA® LM311-DX LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Melt Temperature 177 - 204 °C
350 - 400 °F
Extrusion
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R349AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Melt Temperature 193 - 204 °C
379 - 399 °F
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible)