Material Notes:
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.Designed for thin wall extrusion applications.Recommended for applications requiring excellent flex fatigue resistance.Recommended for applications requiring excellent ozone resistance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
.12 in; ASTM D2240
Tensile Strength at Break 6.62 MPa
960 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 2.69 MPa
390 psi
Across Flow; ASTM D412
Elongation at Break 460 %
460 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Die Temperature 204 °C
400 °F
Extrusion
Melt Temperature 177 - 204 °C
350 - 400 °F
Extrusion
Back Pressure 5.00 - 20.0 MPa
725 - 2900 psi
Extrusion
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 102
Color Natural Color
Form Pellets