| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.45 g/cc | 1.45 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | ASTM D2240 |
| Tensile Strength, Yield | 47.2 MPa | 6850 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.97 GPa | 431 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 87.4 MPa | 12700 psi | ASTM D790 |
| Flexural Modulus | 2.91 GPa | 422 ksi | ASTM D790 |
| Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
| Dart Drop Total Energy | 71.2 J/cm @Temperature 23.0 °C |
0.133 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 156 J/cm @Temperature 23.0 °C |
0.292 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 73.9 °C @Thickness 3.18 mm |
165 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 193 - 204 °C | 379 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| AAMA 303 | Pass | ASTM D4726 |
| Features | High Impact Resistance | |
| Forms | Powder | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| Profile Extrusion | ||
| PVC Cell Classification | 1-42444-33-0101 | ASTM D4216 |
| 16354 | ASTM D1784 | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Building Materials | |
| Fencing & Decking | ||
| Outdoor Applications |