Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
15 sec; ASTM D2240
90
90
ASTM D2240
Tensile Strength at Break 19.3 MPa
2800 psi
510 mm/min; ASTM D638
Tensile Strength 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Oxygen Index 28 %

@Thickness 3.18 mm
28 %

@Thickness 0.125 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 174 - 185 °C
345 - 365 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Additive Biocide
UV Stabilizer
Features Flame Retardant
UV Absorbing
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Users viewing this material also viewed the following: