| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | ASTM D2240 |
| Tensile Strength, Yield | 46.9 MPa | 6800 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.76 GPa | 400 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 95.1 MPa | 13800 psi | ASTM D790 |
| Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
| Izod Impact, Notched | 11.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
20.6 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
| Dart Drop Total Energy | 57.8 J/cm @Temperature 23.0 °C |
0.108 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 200 J/cm @Temperature 23.0 °C |
0.375 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 63.0 µm/m-°C | 35.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 73.9 °C @Thickness 3.18 mm |
165 °F @Thickness 0.125 in |
Compression Molded, Annealed at 50 deg.C; ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | UL 94 |
| 5VA | 5VA | UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 191 - 204 °C | 376 - 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | NSF 51 | The E6950 natural 0000 is the only NSF 51 listed color in this product. |
| Features | Medium Impact Resistance | |
| Forms | Powder | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| PVC Cell Classification | 1-41443-33-0000 | ASTM D4216 |