| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
| Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 31.0 MPa | 4500 psi | ASTM D638 |
| Elongation at Break | 14 % | 14 % | ASTM D638 |
| Flexural Modulus | 1.09 GPa | 158 ksi | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 204 °C | 360 - 400 °F | |
| Mold Temperature | 51.7 - 65.6 °C | 125 - 150 °F | |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |