| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade | 
| Manufacturer | PolyOne Corporation | 
| Trade Name | Geon™ | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D | 82 | 82 | ASTM D2240 | 
| Tensile Strength, Yield | 47.9 MPa | 6950 psi | Type I, 5.1 mm/min; ASTM D638 | 
| Tensile Modulus | 3.09 GPa | 448 ksi | Type I, 5.1 mm/min; ASTM D638 | 
| Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 | 
| Flexural Modulus | 2.88 GPa | 418 ksi | ASTM D790 | 
| Izod Impact, Notched | 13.0           J/cm @Thickness 3.18 mm, Temperature 23.0 °C | 24.4           ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F | Compression Molded; ASTM D256A | 
| Dart Drop Total Energy | 71.2           J/cm @Temperature 23.0 °C | 0.133           ft-lb/mil @Temperature 73.4 °F | Procedure A, C.125; ASTM D4226 | 
| 178           J/cm @Temperature 23.0 °C | 0.333           ft-lb/mil @Temperature 73.4 °F | Procedure B, C.125; ASTM D4226 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ASTM D696 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 71.0           °C @Thickness 3.18 mm | 160           °F @Thickness 0.125 in | Unannealed; ASTM D648 | 
| Flammability, UL94 | V-0 | V-0 | UL 94 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Melt Temperature | 193 - 204 °C | 379 - 399 °F | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| AAMA 303 | Pass | ASTM D4726 | 
| Features | High Impact Resistance | |
| Forms | Powder | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Mean Heat Buildup | 26 °C | ASTM D4803 | 
| Processing Method | Extrusion | |
| Profile Extrusion | ||
| PVC Cell Classification | 1-42444-33-1141 | ASTM D4216 | 
| 16364 | ASTM D1784 | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Building Materials | |
| Fencing & Decking | ||
| Outdoor Applications |