Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7820 GU-N (SEBS) Compound Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 MPa | 100 psi | |
TPI Porene® ABS-SP-100 Super High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Back Pressure | 0.689 - 1.03 MPa | 100 - 150 psi | |
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc.. |
|||
Back Pressure | 0.689 - 1.03 MPa | 100 - 150 psi | |
CTC X-PRO TF 1113 HP Polypropylene Homopolymer, 13% Talc Filled X-PRO TF 1113 HP is a 13% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Back Pressure | 0.689 - 1.03 MPa | 100 - 150 psi | |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Back Pressure | 0.689 - 1.03 MPa | 100 - 150 psi | |
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn .. |
|||
Back Pressure | 0.689 MPa | 100 psi | |
Chi Mei Polylac® PA-747 ABS High impact |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is.. |
|||
Back Pressure | 0.689 MPa | 100 psi | |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Back Pressure | 0.689 MPa | 100 psi | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Back Pressure | 0.689 MPa | 100 psi | |
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Back Pressure | 0.689 - 1.38 MPa | 100 - 200 psi | |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |