Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether) Information provided by PolyOne |
|||
Dry Time | 4.00 hour | 4.00 hour | |
PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
PolyOne Nymax™ GF 1200 A 33 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-GP1 PC/Polyester Alloy High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Dehumidified Dryer; Extrusion |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Dry Time | 4.00 hour | 4.00 hour | Extrusion |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Touch |
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Dry Time | 4.00 hour | 4.00 hour | Extrusion |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |
|||
Dry Time | 4.00 hour | 4.00 hour | |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |