Material Notes:
Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of thermal expansion, which means excellent dimensional stability. Creep resistance is also exceptional. - Natural: DW-1140 NTInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183/A
Filler Content 40 %
40 %
Glass Fiber Reinforcement
Mechanical Properties Metric English Comments
Tensile Strength at Break 253 MPa

@Temperature 23.0 °C
36700 psi

@Temperature 73.4 °F
ISO 527-2
Elongation at Break 2.1 %

@Temperature 23.0 °C
2.1 %

@Temperature 73.4 °F
ISO 527-2
Tensile Modulus 15.5 GPa
2250 ksi
ISO 527-2
Flexural Strength 370 MPa
53700 psi
ISO 178
Flexural Modulus 13.9 GPa

@Temperature 23.0 °C
2020 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 82.0 kJ/m²
39.0 ft-lb/in²
ISO 180
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 297 °C
567 °F
Unannealed; ISO 75-2/Af
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Middle Barrel Temperature 316 - 329 °C
601 - 624 °F
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 150 °C
302 °F
Drying Temperature 120 °C
248 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Descriptive Properties Value Comments
Appearance Natural Color
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Chlorine Resistant
Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Stiffness
High Stiffness
High Strength
High Temperature Strength
Low Moisture Absorption
Forms Pellets
Generic PPA
Processing Method Injection Molding
RoHS Compliance RoHS Compliant
Uses Appliances
Consumer Applications
Filters
Housings
Industrial Applications
Plumbing Parts
Pump Parts
Valves/Valve Parts
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved