| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 6.88 g/cc | 6.88 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 6.89 MPa | 999 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 4.03 GPa | 585 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 12.4 MPa | 1800 psi | ASTM D790 |
| Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Izod Impact, Unnotched (ISO) | 5.25 kJ/m² | 2.50 ft-lb/in² | ASTM D256 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 232 - 271 °C | 450 - 520 °F | |
| Mold Temperature | 37.8 - 48.9 °C | 100 - 120 °F | |
| Drying Temperature | 71.1 °C | 160 °F | |
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Non-Toxic | |
| Forms | Pellets | |
| Generic Material | PEBA-Ether | |
| Generic Name | Polyether Block Amide (PEBA-Ether) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Industrial Applications | |
| Medical/Healthcare Applications | ||
| Projectiles | ||
| Radiation Shielding | ||
| Sporting Goods | ||
| Weighting & Balancing |