Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.6 %

@Thickness 3.18 mm
1.6 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.9 MPa
11300 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 60 %
60 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.55 GPa
370 ksi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C

@Thickness 3.18 mm
140 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Lubricated
Forms Pellets
Generic Material Nylon 6 Alloy
Generic Name Polyamide 6 Alloy (Nylon 6 Alloy)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: