Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dry Time = 6.00 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
PolyOne Bergamid™ A70 G5 T Polyamide 66 (Nylon 66)
Information provided by PolyOne
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Polymer Resources PC/TP-GP3 PC/Polyester Alloy
High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
DAM; Extrusion
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6  (Unverified Data**)
Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Dry Time 3.00 - 6.00 hour
3.00 - 6.00 hour
Injection Molding
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Injection Molding
LG Chemical Lupox® LW5102F PBT+PC+GF10%
Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information..
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Injection Molding
LG Chemical LUPOY HG5000B PC/ABS, Heat Resistance
Description: Injection Molding, PC/ABS, High Gloss, Heat Resistance, High FlowApplication: E&E (housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BFG50-BN00N1 Nylon 6 60% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BPR20-N1 Nylon 6, Flame Retardant (Conditioned)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BTE70-FN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BTE90-DN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour

@Temperature 80.0 °C
2.00 - 6.00 hour

@Temperature 176 °F
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
Dry Time 2.00 - 6.00 hour

@Temperature 80.0 °C
2.00 - 6.00 hour

@Temperature 176 °F
Lanxess Durethan® BKV 130 CS DUS008 600091 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, impact modifiedInformation provided by LANXESS.
Dry Time 2.00 - 6.00 hour

@Temperature 80.0 °C
2.00 - 6.00 hour

@Temperature 176 °F
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber
PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.
Dry Time 2.00 - 6.00 hour

@Temperature 80.0 °C
2.00 - 6.00 hour

@Temperature 176 °F
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber
PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BFG20-FN00N1 Nylon 6 20% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour

@Temperature 80.0 °C
2.00 - 6.00 hour

@Temperature 176 °F
Lanxess Durethan® BKV 115 DUS008 000000 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded
BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Eurotec® Tecodur® PB70 GR30 NL100 HT01 PBT, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec®
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11
Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic..
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
DAM; Injection Molding
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Injection Molding
LG Chemical LUPOY NS5000C PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Copyright © lookpolymers.com All Rights Reserved