Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 185 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 85.0 °C

@Time 14400 sec
185 °F

@Time 4.00 hour
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
Drying Temperature 85.0 °C

@Time 14400 sec
185 °F

@Time 4.00 hour
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
Drying Temperature 85.0 °C

@Time 14400 sec
185 °F

@Time 4.00 hour
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 5202 HS Blend Nylon 66 (Dry)  (discontinued **)
Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as wel..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Injection Molding
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
Drying Temperature 85.0 - 95.0 °C
185 - 203 °F
Injection Molding
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
Drying Temperature 85.0 °C
185 °F
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy
PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc.
Drying Temperature 85.0 °C

@Time 7200 - 10800 sec
185 °F

@Time 2.00 - 3.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info..
Drying Temperature 85.0 °C

@Time 14400 - 28800 sec
185 °F

@Time 4.00 - 8.00 hour
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA)
Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Extrusion
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer
Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer
Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Extrusion
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8202C HS Nylon 6 (Dry)  (discontinued **)
Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)  (discontinued **)
Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also ..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8360 HS 34% Mineral-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8360 HS is a heat stabilized 34% mineral reinforced nylon 6 injection molding resin possessing a high level of toughness and ductility combined with excellent processability and surface aesth..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava..
Drying Temperature 85.0 °C
185 °F
See Materials Notes
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Drying Temperature 85.0 °C
185 °F
Injection
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly..
Copyright © lookpolymers.com All Rights Reserved