Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® SEG7 35% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron SEG7 is an unfilled injection molding type 6 nylon graft copolymer. It has superior impact resistance and flow especially for thinner walled parts and long flow lengths. Copolymerization res.. |
|||
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 1943 is a type 6 nylon graft copolymer developed for injection molding applications requiring improved dry as molded toughness, and increased flexibility. It has an excellent thermal and che.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
(discontinued **) Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The additi.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8200 HS BK-102 is a medium viscosity, heat stabilized, pigmented black, nylon 6 injection molding homopolymer exhibiting resistance to sink-mark formation in thick section, and improved tough.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Drying Temperature | 85.0 °C @Time 7200 - 10800 sec |
185 °F @Time 2.00 - 3.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable .. |
|||
Drying Temperature | 85.0 °C @Time 14400 - 28800 sec |
185 °F @Time 4.00 - 8.00 hour |
|
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA) Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru.. |
|||
Drying Temperature | 85.0 °C | 185 °F | |
Tipco Tipcofil® AG 600 - 30% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 30% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Drying Temperature | 85.0 °C | 185 °F | |
AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, intr.. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Injection |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | Extrusion |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant nylon 6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retard.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8331G HI HS BK-102 Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HI HS BK-102 is a black pigmented, heat stabilized, 30% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as mol.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® GR30 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Drying Temperature | 85.0 °C | 185 °F | See Materials Notes |
BASF Capron® HPN 9233G HS BK-102 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced nylon 6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times .. |
|||
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Drying Temperature | 85.0 °C @Time 14400 sec |
185 °F @Time 4.00 hour |
|
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Drying Temperature | 85.0 °C @Time 14400 - 21600 sec |
185 °F @Time 4.00 - 6.00 hour |
|
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled Injection molding, heat stabilizedInformation provided by PolyPlastic Group. |
|||
Drying Temperature | 85.0 °C @Time 7200 - 14400 sec |
185 °F @Time 2.00 - 4.00 hour |
|
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled Heat stabilizedInformation provided by PolyPlastic Group. |