Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 82.2 - 107 °C | 180 - 225 °F | |
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 75.0 - 107 °C | 167 - 225 °F | Average value: 86.2 °C Grade Count:67 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Drying Temperature | 75.0 - 107 °C | 167 - 225 °F | Average value: 88.7 °C Grade Count:39 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Drying Temperature | 75.0 - 107 °C | 167 - 225 °F | Average value: 85.1 °C Grade Count:16 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Drying Temperature | 75.0 - 107 °C | 167 - 225 °F | Average value: 87.6 °C Grade Count:43 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Drying Temperature | 75.0 - 107 °C | 167 - 225 °F | Average value: 90.1 °C Grade Count:12 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Drying Temperature | 75.0 - 107 °C | 167 - 225 °F | Average value: 85.8 °C Grade Count:6 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Drying Temperature | 79.4 - 107 °C | 175 - 225 °F | Average value: 82.3 °C Grade Count:8 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Drying Temperature | 79.4 - 107 °C | 175 - 225 °F | Average value: 83.6 °C Grade Count:5 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Drying Temperature | 93.0 - 107 °C | 199 - 225 °F | |
PolyOne Lubri-Tech™ NL-000/40T Nylon 6/12 - 40% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 - 107 °C | 199 - 225 °F | |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 - 107 °C | 199 - 225 °F | |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 79.4 - 107 °C | 175 - 225 °F | Average value: 83.9 °C Grade Count:21 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 80.0 - 107 °C | 176 - 225 °F | Average value: 100 °C Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |
|||
Drying Temperature | 80.0 - 107 °C | 176 - 225 °F | Average value: 99.0 °C Grade Count:18 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |