Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PP EIP12030F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPC TS20020 UV Polypropylene Copolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPH T20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPH K5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PPH T5020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 °C | 158 °F | Pre drying temperature |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Drying Temperature | 70.0 °C | 158 °F | Pre drying temperature |
Total Lacqrene® 4240(AS) High Impact Polystyrene
(discontinued **) LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi.. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Drying Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Extrusion Molding |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Drying Temperature | 70.0 °C @Time 14400 sec |
158 °F @Time 4.00 hour |
Pre-dry |
Kingfa FRHIPS-722 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Drying Temperature | 70.0 °C @Time 7200 sec |
158 °F @Time 2.00 hour |
Pre-dry |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Drying Temperature | 70.0 - 90.0 °C @Time 10800 sec |
158 - 194 °F @Time 3.00 hour |
|
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Drying Temperature | 70.0 °C @Time >=7200 sec |
158 °F @Time >=2.00 hour |
|
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Drying Temperature | 70.0 °C | 158 °F | |
Eastman Drystar 0827 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Drying Temperature | 70.0 °C @Time 10800 sec |
158 °F @Time 3.00 hour |
|
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Drying Temperature | 70.0 °C @Time 10800 sec |
158 °F @Time 3.00 hour |
|
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 70.0 - 75.0 °C @Time 14400 sec |
158 - 167 °F @Time 4.00 hour |
|
Chi Mei Acryrex® CM-211 PMMA Features:Good Weather ResistanceHigh ClarityHigh FlowHigh GlossHigh Heat ResistanceHigh ViscosityUses:ContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: Pellets.. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Pre-drying Temperature |
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Polykemi AB POLYfill PP 150ENH Polypropylene, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Drying Temperature | 70.0 °C | 158 °F | Desiccant Dryer |
ExxonMobil Santoprene® 8291-80TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |