Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.022 - 0.024 cm/cm

@Thickness 4.00 mm
0.022 - 0.024 in/in

@Thickness 0.157 in
E2P method
Melt Flow 8.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break 15 %
15 %
ISO 527
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Izod Impact, Notched (ISO) 2.80 kJ/m²
1.33 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 225 - 250 °C
437 - 482 °F
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour