Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 254 °C | 490 °F | |
Nilit Polynil® N66-P50N Lubed Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PC-G5-IM Polycarbonate, 5% Glass Reinforced, Impact Modified, Foamable Polycarbonate, 5% Glass Reinforced, Impact Modified, FoamableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Rear Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Rear Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Rear Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Rear Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Rear Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Rear Barrel Temperature | 254 - 271 °C | 490 - 520 °F | |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G43HL 43% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 °C | 490 °F | |
PTS Trimid® N66-S100L High Impact Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 271 °C | 490 - 520 °F | |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Rear Barrel Temperature | 254 - 274 °C | 490 - 525 °F | |
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 254 - 282 °C | 490 - 540 °F | |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |