Processing Properties Metric English Comments
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc.
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Oxford Polymers PC 714-FR Series PC, Flame retardant
Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-GP1 General Purpose Nylon 66
General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized
General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized
General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized
Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. ..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-MD-[color]-H Nylon 66, 2% MoS2
Nylon 66, 2% Molybdenum Disulfide for Lubrication and Wear, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 254 - 277 °C
490 - 530 °F
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow
Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Rear Barrel Temperature 254 - 277 °C
490 - 530 °F
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow
Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated
General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified
Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-IM1-[color]-H Nylon 66, Medium Impact Modified, Heat Stabilized
Nylon 66, Medium Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Ny..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Polymer Resources NY66-MD2 Nylon 66, 2% MoS2
Nylon 66, 2% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Mitsubishi Iupilon® S2000R 9.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 266 - 277 °C
510 - 530 °F
Mitsubishi Iupilon® S2001R 9.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 260 - 277 °C
500 - 530 °F
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Copyright © lookpolymers.com All Rights Reserved