Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 193.1 MPa
28010 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 251 °C
484 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 254 °C
490 °F
Middle Barrel Temperature 268 °C
515 °F
Front Barrel Temperature 285 °C
545 °F
Nozzle Temperature 266 - 282 °C
510 - 540 °F
Melt Temperature 271 - 293 °C
520 - 560 °F
Mold Temperature 26.7 - 93.3 °C
80.0 - 200 °F
Drying Temperature 71.1 °C
160 °F
Dry Time 4 hour
4 hour
Injection Pressure 68.9 MPa
10000 psi
Back Pressure 0.0689 - 0.689 MPa
10.0 - 100 psi
Screw Speed 30 - 60 rpm
30 - 60 rpm