| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized | 
| Manufacturer | Polymer Technology & Services, LLC (PTS) | 
| Trade Name | Trimid® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 57.2 MPa | 8300 psi | ASTM D638 | 
| Elongation at Break | 48 % | 48 % | ASTM D638 | 
| Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 | 
| Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 | 
| Izod Impact, Notched |           1.33           J/cm           @Thickness 3.17 mm  | 
                  2.49           ft-lb/in           @Thickness 0.125 in  | 
        ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 254 °C | 489 °F | ASTM D789 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Rear Barrel Temperature | 254 °C | 490 °F | |
| Middle Barrel Temperature | 268 °C | 515 °F | |
| Front Barrel Temperature | 285 °C | 545 °F | |
| Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
| Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
| Mold Temperature | 26.7 - 93.3 °C | 80.0 - 200 °F | |
| Drying Temperature | 71.1 °C | 160 °F | |
| Dry Time | 4 hour | 4 hour | |
| Injection Pressure | 68.9 MPa | 10000 psi | |
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm |