| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | CP-Polymer-Technik GmbH & Co. |
| Trade Name | Wellamid® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Conditioned.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 1.8 - 2.5 % | 1.8 - 2.5 % | 23°C/50%RH, Starting when dry; DIN 53495 |
| Linear Mold Shrinkage | 0.0050 cm/cm @Thickness 4.00 mm |
0.0050 in/in @Thickness 0.157 in |
|
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm @Thickness 4.00 mm |
0.0060 in/in @Thickness 0.157 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 5.0 % | 5.0 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
| Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 255 °C | 491 °F | Kofler |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 93 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
| Dielectric Constant | 6.0 @Frequency 1e+6 Hz |
6.0 @Frequency 1e+6 Hz |
IEC 250 |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
| Dielectric Loss Index | 0.10 | 0.10 | At 1 MHz; IEC 250 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
| Mold Temperature | 80.0 - 100 °C | 176 - 212 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Holding Pressure | Medium | |
| Injection Speed | Medium to High | |
| Screw Speed | Medium |