Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 150 °C | 302 °F | |
PolyOne OnForce™ LFT SF-40LGF/001 Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Mold Temperature | 150 °C | 302 °F | DAM; optimum |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8124 Polyether imide, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8148 PPS, linear, with PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be.. |
|||
Mold Temperature | 150 - 190 °C | 302 - 374 °F | |
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Mold Temperature | 150 - 170 °C | 302 - 338 °F | |
LATI Laramid CE/60 PPA, 60% Mineral Reinforced Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Mold Temperature | 150 - 170 °C | 302 - 338 °F | |
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Mold Temperature | 150 °C | 302 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Mold Temperature | 150 °C | 302 °F | |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Mold Temperature | 150 - 190 °C | 302 - 374 °F | Injection molding |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Mold Temperature | 150 - 190 °C | 302 - 374 °F | Injection molding |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |
|||
Mold Temperature | 150 - 175 °C | 302 - 347 °F | |
Resinoid 2018 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 150 °C | 302 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |