Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinoid 2018 Phenolic Molding, Fabric Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Fabric Filled
Manufacturer Resinoid
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinoid 2018 Phenolic Molding, Fabric Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792A
Water Absorption 0.77 %
0.77 %
24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Positive Mold; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ASTM D651
Flexural Strength 128 MPa
18600 psi
ASTM D790
Compressive Strength 152 MPa
22000 psi
ASTM D695
Izod Impact, Notched 0.945 J/cm
1.77 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 10.4 kV/mm
264 kV/in
Short Time; Dry; ASTM D149
Processing Properties Metric English Comments
Mold Temperature 150 - 175 °C
302 - 347 °F