Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 2205 Phenolic Molding, Cellulose Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 165 - 180 °C | 329 - 356 °F | |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Mold Temperature | 121 - 180 °C | 250 - 356 °F | Average value: 152 °C Grade Count:48 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Mold Temperature | 135 - 180 °C | 275 - 356 °F | Average value: 163 °C Grade Count:36 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | Compression molding |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | |
Eurotec® Tecomid® NT40 MR40 NL HS PPA, 40% mineral reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st.. |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 1324 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 2020 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 7051 SS Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |