Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 1382 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 2011 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 2225 Phenolic Molding, Cellulose Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Mold Temperature | 65.6 - 180 °C | 150 - 356 °F | Average value: 155 °C Grade Count:20 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be.. |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | |
Eurotec® Tecomid® NT40 MR40 NL HS PPA, 40% mineral reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Mold Temperature | 130 - 180 °C | 266 - 356 °F | Injection molding |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | Injection molding |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | Injection molding |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | Injection molding |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Mold Temperature | 160 - 180 °C | 320 - 356 °F | |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 1324 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Mold Temperature | 155 - 180 °C | 311 - 356 °F | |
Resinoid 7051 SS Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Mold Temperature | 150 - 180 °C | 302 - 356 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |