Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 79.4 - 98.9 °C | 175 - 210 °F | |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Mold Temperature | 71.1 - 98.9 °C | 160 - 210 °F | |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Mold Temperature | 71.1 - 98.9 °C | 160 - 210 °F | |
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 6/6, 35% Fiberglass (DAM)
(discontinued **) Information provided by Ravago. |
|||
Mold Temperature | 71.1 - 98.9 °C | 160 - 210 °F | |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 71.1 - 98.9 °C | 160 - 210 °F | |
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F