Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
Water Absorption | 0.40 % | 0.40 % | 24 hrs; ASTM D570 |
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | 0.125 in; ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 82 | 82 | ASTM D785 |
Tensile Strength at Break | 117 MPa | 17000 psi | ASTM D638 |
Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
Flexural Strength | 193 MPa | 28000 psi | ASTM D790 |
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F; ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 249 °C | 480 °F | Unannealed; ASTM D648 |
Flammability, UL94 | HB | HB | 0.0591 in, BK |
HB | HB | 0.118 in, BK |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Dielectric Strength | 21.7 kV/mm | 550 kV/in | ASTM D149 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
Drying Temperature | 73.9 °C | 165 °F | |
Dry Time | 2 - 4 hour | 2 - 4 hour | |
Moisture Content | 0.18 % | 0.18 % | |
Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
Screw Speed | 40 - 120 rpm | 40 - 120 rpm |
Descriptive Properties | Value | Comments |
---|---|---|
Holding Pressure | 750 to 1400 psi | |
Injection Rate | Fast |