| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
| Water Absorption | 0.60 % | 0.60 % | 24 hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | 0.125 in; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 94 | 94 | ASTM D785 |
| Tensile Strength at Break | 96.5 MPa | 14000 psi | ASTM D638 |
| Elongation at Break | 1.5 % | 1.5 % | ASTM D638 |
| Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
| Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
| Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | 73°F; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 48.6 µm/m-°C <br>@Temperature 20.0 °C |
27.0 µin/in-°F <br>@Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 238 °C | 460 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 193 °C | 380 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | HB | HB | 0.0590 in, BK |
| HB | HB | 0.0590 in, NC | |
| HB | HB | 0.118 in, BK | |
| HB | HB | 0.118 in, NC |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.9 <br>@Frequency 100 Hz |
3.9 <br>@Frequency 100 Hz |
ASTM D150 |
| Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
| Mold Temperature | 65.6 - 98.9 °C | 150 - 210 °F | |
| Drying Temperature | 73.9 °C | 165 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Moisture Content | 0.20 % | 0.20 % | |
| Back Pressure | 0.138 - 0.414 MPa | 20.0 - 60.0 psi | |
| Screw Speed | 40 - 120 rpm | 40 - 120 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Injection Rate | Fast |