Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delive.. |
|||
Mold Temperature | 60.0 - 87.8 °C | 140 - 190 °F | |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Mold Temperature | 60.0 - 107 °C | 140 - 225 °F | |
PolyOne Nymax™ GF 1204 33 MS 2 Grey A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection Molding |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Mold Temperature | 60.0 - 110 °C | 140 - 230 °F | |
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab.. |
|||
Mold Temperature | 60.0 °C | 140 °F | |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
CP-Polymer-Technik Wellamid® 6000 GS 15 HWCP 15% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural Information provided by Eurotec® |
|||
Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy Non Halogen Flame Retardant, High FlowInformation provided by E-Polymers Co. Ltd. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | 80 - 90°C is recommended |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | 80 - 90°C is recommended |
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced 40% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection-molding |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Conditioned) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Mold Temperature | 60.0 °C | 140 °F | Optimal |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection molding |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |