Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
DAM; ASTM D792
Water Absorption 1.1 %
1.1 %
24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
0.125 in, DAM; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Flexural Strength 28.3 MPa
4100 psi
ASTM D790
Flexural Modulus 0.614 GPa
89.0 ksi
ASTM D790
Izod Impact, Notched NB
NB
73°F; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 243 - 271 °C
470 - 520 °F
Mold Temperature 60.0 - 87.8 °C
140 - 190 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.18 %
0.18 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 40 - 120 rpm
40 - 120 rpm