Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 246 - 288 °C | 475 - 550 °F | |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 246 - 288 °C | 475 - 550 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Nozzle Temperature | 249 - 288 °C | 480 - 550 °F | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Nozzle Temperature | 246 - 288 °C | 475 - 550 °F | |
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 266 - 288 °C | 510 - 550 °F | |
LTL Color Compounds ColorFast® PC200 Polycarbonate 20 melt superior processing, fast cyclingAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Nozzle Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Nozzle Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow Information provided by Star Plastics, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 277 - 288 °C | 530 - 550 °F | |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |