Processing Properties Metric English Comments
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 1008 T Polypropylene
Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 1012 C Polypropylene
Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 1020 C Polypropylene
Calcium Carbonate Filler, 10% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 3014 CUW Polypropylene
Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 3018 TU Polypropylene
Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 4006 TH Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 4015 THW Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 4518 CUW Polypropylene
Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 5014 CUW Polypropylene
Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 2003 TI Polypropylene
Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 193 - 227 °C
380 - 440 °F
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Nozzle Temperature 193 °C
380 °F
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys..
Nozzle Temperature 193 - 221 °C
380 - 430 °F
LTL Color Compounds ColorFast® FRA202 General Purpose ABS
General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 193 - 221 °C
380 - 430 °F
LTL Color Compounds ColorFast® FRA203 ABS
Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer
Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer
Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer
Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer
Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 193 - 232 °C
380 - 450 °F
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer
Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer
Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc..
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer
Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Multibase Multi-Pro® 4007 XGS Polypropylene
Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase
Nozzle Temperature 193 - 232 °C
380 - 450 °F
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Nozzle Temperature 193 - 227 °C
380 - 440 °F
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Copyright © lookpolymers.com All Rights Reserved