Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 1012 C Polypropylene Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 2518 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 2518 TU Polypropylene Talc Filled, 25% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 4017 C Polypropylene Calcium Carbonate Filler, 40% by weight.Features:Stiffness, Good Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Nozzle Temperature | 193 - 224 °C | 379 - 435 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Nozzle Temperature | 193 - 224 °C | 379 - 435 °F | |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 - 221 °C | 380 - 430 °F | |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2860L Thermoplastic Elastomer Elastocon® 2860L thermoplastic elastomer has been developed for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 2860L is FDA compliant and well s.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is.. |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Nozzle Temperature | 193 - 227 °C | 380 - 440 °F | |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Nozzle Temperature | 193 - 204 °C | 380 - 400 °F | |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |
|||
Nozzle Temperature | 193 - 232 °C | 380 - 450 °F | |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |