Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® CLR40 can be overmolded onto polypropylene.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
ASTM D2240
Tensile Strength 6.50 MPa
943 psi
ASTM D412
Elongation at Break 728 %
728 %
ASTM D412
100% Modulus 0.00142 GPa
0.206 ksi
ASTM D412
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 177 °C
330 - 350 °F
Front Barrel Temperature 182 - 188 °C
360 - 370 °F
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi
Descriptive Properties Value Comments
Injection Rate Fast
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved