Material Notes:
Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 2840 can be overmolded onto polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength, Yield 5.54 MPa
804 psi
ASTM D412
Elongation at Break 576 %
576 %
ASTM D412
100% Modulus 0.000958 GPa
0.139 ksi
ASTM D412
Compression Set 23 %

@Time 79200 sec
23 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 177 °C
330 - 350 °F
Front Barrel Temperature 182 - 188 °C
360 - 370 °F
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi