Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Nilit Polynil® N66-P300 High Viscosity Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Nilit Polynil® N66-P50N Lubed Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-1010L Lubed, Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-SG33-BK 33% Glass Reinforced, High Impact Black Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 260 - 282 °C | 500 - 540 °F | |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Nozzle Temperature | 271 - 282 °C | 520 - 540 °F | |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Nozzle Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Beetle® 140 BH Nylon 66, Glass Bead Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Nozzle Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS.. |
|||
Nozzle Temperature | 268 - 282 °C | 515 - 540 °F | |
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302.. |
|||
Nozzle Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Nozzle Temperature | 254 - 282 °C | 490 - 540 °F | |
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman. |
|||
Nozzle Temperature | 271 - 282 °C | 520 - 540 °F | |
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Nozzle Temperature | 271 - 282 °C | 520 - 540 °F | |
Wellman Wellamid® FRGF25-66-N Flame Retardant Nylon 66, Lubricated, 25% Glass Fiber Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Nozzle Temperature | 268 - 282 °C | 515 - 540 °F | |
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Nozzle Temperature | 243 - 282 °C | 469 - 540 °F | Average value: 256 °C Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |