Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | |
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive.. |
|||
Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP1 PC/Polyester Alloy High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Front Barrel Temperature | 260 - 295 °C | 500 - 563 °F | Start Point: 280°C |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-G15 15% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-MG45 45% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA), 30% Glass Fiber Ixef® 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance.Features: .. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE