Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 1505 R Polypropylene Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 2004 R Polypropylene Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided .. |
|||
Front Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Front Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Front Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Front Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Front Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Front Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Start Point: 240°C |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Front Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Injection Molding |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Front Barrel Temperature | 245 - 260 °C | 473 - 500 °F | Injection Molding |
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40%Glass Filled, High Impact LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Front Barrel Temperature | 225 - 260 °C | 437 - 500 °F | Injection Molding |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Front Barrel Temperature | 225 - 260 °C | 437 - 500 °F | Injection Molding |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Front Barrel Temperature | 245 - 260 °C | 473 - 500 °F | Injection Molding |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Front Barrel Temperature | 190 - 260 °C | 374 - 500 °F | Injection |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Front Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Start Point: 240°C |
Kingfa MAC-451PG Electroplating PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank coverComputer and accessor.. |
|||
Front Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |