| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
| Multibase Multi-Pro® 2516 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult.. |
|||
| Middle Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
| Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
| Middle Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
| Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
| Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
| RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
| RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products HP521-501UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 149B Shale Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products HP522-390 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, AYCA Medium Prairie Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
| Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
| Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
| PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
| Middle Barrel Temperature | 199 °C | 390 °F | Injection |
| Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
| Middle Barrel Temperature | 199 °C | 390 °F | |
| ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
| Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
| Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,.. |
|||
| Middle Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
| Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
| Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
| Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||