Processing Properties Metric English Comments
Middle Barrel Temperature 260 - 275 °C
500 - 527 °F
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Middle Barrel Temperature 260 - 275 °C
500 - 527 °F
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Middle Barrel Temperature 260 - 275 °C
500 - 527 °F
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Middle Barrel Temperature 260 - 275 °C
500 - 527 °F
Injection Molding
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant
Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical
Middle Barrel Temperature 260 - 275 °C
500 - 527 °F
Injection Molding
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity
Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact
Feature: Injection Molding, PA6+MF23%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Middle Barrel Temperature 260 - 275 °C
500 - 527 °F
Injection Molding
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem..
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY GP5006B PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
LG Chemical LUPOY HI-1002 High Impact Modified PC, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY HR5007AE PC/ABS, High Impact
Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY NS5000 PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Middle Barrel Temperature 235 - 275 °C
455 - 527 °F
Injection Molding
LG Chemical LUPOY SG5009F PC/ABS
Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced
Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant
Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 615 HP PET 15% Glass Reinforced
Vypet VNT 615HP is a modified 15% fiberglass reinforced PET injection molding compound designed for automotive structural applications.Features: Easy, fast processing; Excellent strength and stiffne..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 645 PET 45% Glass Reinforced
Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced
Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 840 HY PET 40% Glass-Mineral Reinforced
Vypet VNT 840 HY is a 40% glass/mineral reinforced PET high strength injection molding compound with improved hydrolysis stability designed for electrical and structural applications, with High Diel..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced
Vypet VNT 840 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric Strength Features: High temperature performan..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 930 PET 30% Glass Reinforced
Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent..
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Zone 2
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded
AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Zone 2
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym..
Middle Barrel Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY NS5000C PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical