Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 243 - 266 °C | 469 - 511 °F | |
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Middle Barrel Temperature | 243 - 266 °C | 469 - 511 °F | |
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Middle Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Middle Barrel Temperature | 235 - 266 °C | 455 - 510 °F | |
Diamond Polymers ABS/PC 9901 Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 260 - 266 °C | 500 - 510 °F | |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 235 - 266 °C | 455 - 511 °F | |
A. Schulman ComAlloy Hiloy® 242 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 266 °C | 455 - 511 °F | |
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 266 °C | 455 - 511 °F | |
A. Schulman ComAlloy Hiloy® 247 SAN, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 246 - 266 °C | 475 - 511 °F | |
A. Schulman ComAlloy Hiloy® 263 Glass Reinforced, Modified SMA Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 266 °C | 455 - 510 °F | |
Diamond Polymers ABS/PC 9801 Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc. |