Material Notes:
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Ultimate 84.0 MPa
12200 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 123 MPa
17800 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.49 J/cm
2.79 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F