Material Notes:
Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Exceptional Colorability - Outstanding Adhesion in Both Two-Shot and Insert Molding Processes - Soft, Rubbery Grip - Very Easy to ProcessPurge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Versaflex™ OM 6059-9 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versaflex™ OM 6059-9 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 3 to 6 in/sec 1st Stage - Boost Pressure: 300 to 800 psi 2nd Stage - Hold Pressure: 0% of Boost Hold Time (Thick Part): 0 to 4 sec Hold Time (Thin Part): 0 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Viscosity 16900 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
16900 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
75000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
75000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
10 sec; ASTM D2240
Tensile Strength at Break 2.45 MPa

@Temperature 23.0 °C
355 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 1.75 MPa

@Strain 100 %,
Temperature 23.0 °C
254 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 290 %

@Temperature 23.0 °C
290 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Compression Set 14 %

@Temperature 22.0 °C,
Time 79200 sec
14 %

@Temperature 71.6 °F,
Time 22.0 hour
ASTM D395B
63 %

@Temperature 70.0 °C,
Time 79200 sec
63 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 204 °C
360 - 399 °F
Middle Barrel Temperature 243 - 266 °C
469 - 511 °F
Front Barrel Temperature 249 - 271 °C
480 - 520 °F
Nozzle Temperature 254 - 277 °C
489 - 531 °F
Melt Temperature 249 - 271 °C
480 - 520 °F
Mold Temperature 12.8 - 29.4 °C
55.0 - 84.9 °F
Back Pressure 0.000 - 0.552 MPa
0.000 - 80.1 psi
Screw Speed 80 - 120 rpm
80 - 120 rpm
Descriptive Properties Value Comments
Agency Ratings UL 94 .QMFZ2.E76261
Appearance Black
Features Good Adhesion
Good Colorability
Good Processability
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Suggested Max Regrind 20%
Users viewing this material also viewed the following: