Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 204 - 260 °C | 400 - 500 °F | |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Middle Barrel Temperature | 249 - 260 °C | 480 - 500 °F | |
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 235°C |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
LG Chemical LUMID GP1300A(W) PA6, High Viscosity Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Injection Molding |
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided .. |
|||
Middle Barrel Temperature | 245 - 260 °C | 473 - 500 °F | Injection Molding |
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5000SP PBT+PC Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® TE5100 PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, High Impact resistant, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 30965-26-5, 103598-77-2 and 65997-17-3Information provided.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Middle Barrel Temperature | 249 - 260 °C | 480 - 500 °F | |
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1020 Polyester-PC Alloy The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 255°C |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Middle Barrel Temperature | 246 - 260 °C | 475 - 500 °F | |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 241 - 260 °C | 465 - 500 °F | |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika AXF-1500-05 Conditioned Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika AXG-1500-300 Conditioned Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika LM-8503-10 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |