Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Middle Barrel Temperature | 243 - 271 °C | 470 - 520 °F | |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |